Micrograph no
507
Brief description
Annealed 5% Sn bronze.
Keywords
alloy Link to MATTER Glossary entry for alloy, annealing Link to MATTER Glossary entry for annealing, bronze Link to MATTER Glossary entry for bronze, copper, metal, tin
Categories
Metal or alloy
System
Cu-Sn   Link to phase diagram
Composition
Cu 95, Sn 5 (wt%),
Standard codes
Reaction
Processing
Cast annealed 700 ºC for 24 hrs
Applications
Sample preparation
Ferric chloride
Technique
Reflected light microscopy
Length bar
200 μm
Further information
A good example of the creation of annealing twins.
Contributor
Dr R F Cochrane
Organisation
Department of Materials, University of Leeds
Date
04/09/02
Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International
Related micrographs