Brief description
Ti, Al 6, V 4 (wt%), Widmanstätten microstructure
Keywords
alloy Link to MATTER Glossary entry for alloy, aluminium Link to MATTER Glossary entry for aluminium, metal, titanium, vanadium, Widmanstätten Link to MATTER Glossary entry for Widmanstätten
Categories
Metal or alloy
System
Ti-Al-V
Composition
Ti, Al 6, V 4 (wt%)
Standard codes
Reaction
Processing
Applications
Sample preparation
Technique
Reflected light microscopy
Length bar
400 μm
Further information
This sample is a mixed α+β Ti alloy with a Widmanstätten microstructure. The α phase (h.c.p) precipitates out as Widmanstätten plates upon cooling from the β phase (b.c.c). The matrix (dark) appears as thin layers between the a plates (light). The crystallographic relationships are very precise in this example giving h.c.p α plates in a b.c.c β matrix.
Contributor
Prof T W Clyne
Organisation
Department of Materials Science and Metallurgy, University of Cambridge
Date
25/10/01
Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International