DoITPoMS Micrograph Library Full Record for Micrograph 705

Full Record for Micrograph 705

Link to full size image of micrograph 705
[119 KB]

View micrograph
.. in new window

View micrograph and record
.. in new window


You can also view and download the micrographs on Flickr
Micrograph no
705
Brief description
Cu-? wt% P
Keywords
alloy Link to MATTER Glossary entry for alloy, copper, dendrite Link to MATTER Glossary entry for dendrite, metal, phosphorus Link to MATTER Glossary entry for phosphorus
Categories
Metal or alloy
System
Cu-P   Link to phase diagram
Composition
Not specified
Standard codes
Reaction
Processing
Applications
Sample preparation
Technique
Reflected light microscopy
Length bar
400 μm
Further information
Contributor
Dr J Marrow
Organisation
Department of Materials Science, University of Manchester and UMIST
Date
07/11/02
Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International