23 micrographs for keyword hypoeutectoid, ordered by micrograph number.


Showing 1 - 10 of 23 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 17 Micrograph 17 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 18 Micrograph 18 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 19 Micrograph 19 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Scanning electron microscopy (SEM)
30 μm
Link to full record for micrograph 20 Micrograph 20 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 225 Micrograph 225 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 226 Micrograph 226 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 227 Micrograph 227 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 228 Micrograph 228 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 229 Micrograph 229 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 230 Micrograph 230 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.5 (wt%)
Reflected light microscopy
200 μm

Showing 1 - 10 of 23 micrographs Page 1 2 3 | Previous | Next