Link to full record for micrograph 374 Micrograph 374 : Fully transformed ledeburite cast iron
System: Fe-C-X, Composition: Fe, C 4.17, Si 0.40, Mn 0.45, Cr 0.95 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 375 Micrograph 375 : Fully transformed ledeburite cast iron
System: Fe-C-X, Composition: Fe, C 4.17, Si 0.40, Mn 0.45, Cr 0.95 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 378 Micrograph 378 : Grey cast iron with significant Si content
System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 379 Micrograph 379 : Grey cast iron with significant Si content
System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 380 Micrograph 380 : Grey cast iron with significant Si content
System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 381 Micrograph 381 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
400 μm
Link to full record for micrograph 382 Micrograph 382 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
200 μm
Link to full record for micrograph 383 Micrograph 383 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
100 μm
Link to full record for micrograph 387 Micrograph 387 : Silal
System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal)
Reflected light microscopy
400 μm
Link to full record for micrograph 388 Micrograph 388 : Silal
System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal)
Reflected light microscopy
200 μm