Link to full record for micrograph 582 Micrograph 582 : Low magnification SEM image of open cell polyurethane foam
System: Polyurethane (PU), Composition: Not specified
Scanning electron microscopy (SEM)
4 mm
Link to full record for micrograph 583 Micrograph 583 : SEM image of Velcro (TM)
System: Nylon, Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 584 Micrograph 584 : External surface of blow-moulded HDPE
System: High density polyethylene (HDPE), Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 585 Micrograph 585 : Internal surface of blow-moulded HDPE
System: High density polyethylene (HDPE), Composition: Not specified
Scanning electron microscopy (SEM)
6 μm
Link to full record for micrograph 586 Micrograph 586 : Fracture surface in polystyrene
System: Polystyrene (PS), Composition: Not specified
Scanning electron microscopy (SEM)
160 μm
Link to full record for micrograph 587 Micrograph 587 : Parabolic beach marks on a polystyrene fracture surface
System: Polystyrene (PS), Composition: Not specified
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 588 Micrograph 588 : Beach marks on a polystyrene fracture surface
System: Polystyrene (PS), Composition: Not specified
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 589 Micrograph 589 : Remnants of crazes on a polystyrene fracture surface
System: Polystyrene (PS), Composition: Not specified
Scanning electron microscopy (SEM)
8 μm
Link to full record for micrograph 590 Micrograph 590 : Remnants of crazes on a polycarbonate fracture surface
System: Polycarbonate (PC), Composition: Not specified
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 591 Micrograph 591 : Crazing near a fracture surface in polycarbonate
System: Polycarbonate (PC), Composition: Not specified
Scanning electron microscopy (SEM)
80 μm