Link to full record for micrograph 592 Micrograph 592 : The tip of a craze in polycarbonate
System: Polycarbonate (PC), Composition: Not specified
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 593 Micrograph 593 : Ductile tearing near a fracture surface in polycarbonate
System: Polycarbonate (PC), Composition: Not specified
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 594 Micrograph 594 : Carbon string
System: C, Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 595 Micrograph 595 : Thermoset case of an electrical plug
System: Urea formaldehyde, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 596 Micrograph 596 : Glass-fibre reinforced polymer
System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres
Reflected light microscopy
400 μm
Link to full record for micrograph 597 Micrograph 597 : Frozen stress photoelastic fringe pattern during fibre pushout
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 598 Micrograph 598 : Frozen stress photoelastic assessment of load distribution around a cylinder
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 599 Micrograph 599 : Frozen stress photoelastic assessment of load distribution around an ellipsoid
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 600 Micrograph 600 : Spherulite in poly-3-hydroxy butyrate (PHB)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Cross-polarised light microscopy
1 μm
Link to full record for micrograph 601 Micrograph 601 : Spherulites in in poly-3-hydroxy butyrate (PHB)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Cross-polarised light microscopy
240 nm