Link to full record for micrograph 639 Micrograph 639 : Twist-escaped loops in the liquid crystalline polymer MBBA
System: Liquid crystalline polymer, Composition: MBBA
Cross-polarised light microscopy
200 μm
Link to full record for micrograph 640 Micrograph 640 : Fracture surface in a liquid crystalline polymer, oriented by a magnetic field
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 641 Micrograph 641 : Fracture surface in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401
Scanning electron microscopy (SEM)
12 μm
Link to full record for micrograph 642 Micrograph 642 : Fracture surface in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402
Scanning electron microscopy (SEM)
12 μm
Link to full record for micrograph 643 Micrograph 643 : Aligned carbon nanotubes, coated with a conducting polymer
System: Carbon nanotube, Composition: Coating of polypyrrole
Scanning electron microscopy (SEM)
1 μm
Link to full record for micrograph 644 Micrograph 644 : Carbon nanotubes, coated with a conducting polymer
System: Carbon nanotube, Composition: Coating of polypyrrole
Scanning electron microscopy (SEM)
100 nm
Link to full record for micrograph 645 Micrograph 645 : An image of a single crystal alkane
System: Alkane, Composition: C294H590
Transmission electron microscopy (TEM)
2.4 μm
Link to full record for micrograph 646 Micrograph 646 : Spherulite growth imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
500 nm
Link to full record for micrograph 647 Micrograph 647 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
3 μm
Link to full record for micrograph 648 Micrograph 648 : A spherulite imaged by atomic force microscopy (AFM)
System: Polyhydroxybutyrate (PHB), Composition: Not specified
Atomic force microscopy (AFM)
2 μm