System
333 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 291 - 300 of 333 micrographs | Page 1 .. 27 28 29 30 31 32 33 34 | Previous | Next |
Micrograph
805
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, V 5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
|
Micrograph
807
:
Martensitic steel solution treated and rapidly cooled with dislocation in retained autenite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
808
:
Martensitic steel tempered with precipitation of Mo2C System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 200 nm |
|
Micrograph
809
:
Austenitic stainless steel solution treated, quenched, deformed in tension, then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
810
:
Ferritic steel heat treated and water quenched System: Fe-C-X, Composition: Fe, Mn 1, S 0.02 (wt%) Scanning electron microscopy (SEM) 1.5 μm |
|
Micrograph
811
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
812
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
813
:
Austenitic stainless steel solution treated, quenched and tempered, with M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
|
Micrograph
814
:
Austenitic stainless steel solution treated, quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
Showing 291 - 300 of 333 micrographs | Page 1 .. 27 28 29 30 31 32 33 34 | Previous | Next |