System
333 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 301 - 310 of 333 micrographs | Page 1 .. 28 29 30 31 32 33 34 | Previous | Next |
Micrograph
815
:
Martensitic steel, lightly rolled, with dislocations in austenite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Scanning electron microscopy (SEM) 400 nm |
|
Micrograph
816
:
Austenitic stainless steel solution treated, quenched and tempered, showing M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
|
Micrograph
817
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1 Scanning electron microscopy (SEM) 2 μm |
|
Micrograph
818
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 2.5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
819
:
Austenitic stainless steel water quenched then deformed in impact System: Fe-C-X, Composition: Stainless steel with Cr 13.7, Mn 14.2, C 0.12 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
820
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 5, C O.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
821
:
Austenitic stainless steel impact deformed at room temperature System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%) Scanning electron microscopy (SEM) 2.5 μm |
|
Micrograph
822
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
|
Micrograph
823
:
Martensitic steel tempered, with dislocation helices in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
824
:
Martensitic steel tempered, with precipitation of Mo2C in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
Showing 301 - 310 of 333 micrographs | Page 1 .. 28 29 30 31 32 33 34 | Previous | Next |