System
333 micrographs for system Fe-C-X, ordered by micrograph number.
Showing 311 - 320 of 333 micrographs | Page 1 .. 28 29 30 31 32 33 34 | Previous | Next |
Micrograph
826
:
Austenitic stainless steel tempered, with Mo2 and M6C precipitates System: Fe-C-X, Composition: Fe, C 0.20, Mo 3.8, Ta 0.22 (wt%) Scanning electron microscopy (SEM) 2.5 μm |
|
Micrograph
827
:
Martensitic steel quenched then tempered System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
828
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
829
:
Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
830
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 2 μm |
|
Micrograph
831
:
Austenitic stainless steel water quenched, with a-martensite needles within lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
832
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 200 nm |
|
Micrograph
833
:
Austenitic stainless steel solution treated, quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
834
:
Steel slowly cooled, fracture surface of commercial ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
835
:
Martensitic steel tempered, with precipitation of Mo2C System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
Showing 311 - 320 of 333 micrographs | Page 1 .. 28 29 30 31 32 33 34 | Previous | Next |