331 micrographs for system Fe-C-X, ordered by micrograph number.


Showing 31 - 40 of 331 micrographs Page 1 2 3 4 5 6 7 .. 34 | Previous | Next

Link to full record for micrograph 73 Micrograph 73 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 78 Micrograph 78 : Forging steel, brittle, intergranular fracture
System: Fe-C-X, Composition: Forging steel
Scanning electron microscopy (SEM)
800 μm
Link to full record for micrograph 133 Micrograph 133 : Steel, austenitised at 1200 centigrade for 120 s and then transformed isothermally at 350 centigrade for 2000 s before cooling to room temperature.
System: Fe-C-X, Composition: Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%)
Atomic force microscopy (AFM)
1 μm
Link to full record for micrograph 134 Micrograph 134 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
600 nm
Link to full record for micrograph 135 Micrograph 135 : High carbon steel
System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%)
Transmission electron microscopy (TEM)
1.5 μm
Link to full record for micrograph 143 Micrograph 143 : Notched low carbon ferritic steel, failed through cleavage.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 146 Micrograph 146 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 147 Micrograph 147 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 201 Micrograph 201 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
400 μm
Link to full record for micrograph 202 Micrograph 202 : Normalised low carbon steel, showing directionality
System: Fe-C-X, Composition: Wrought iron (plain carbon steel)
Reflected light microscopy
200 μm