Here, both reactions are under activation control - they
go at the rate predicted by the Tafel analysis.
Click to see what happens when oxygen is limited
This effect is useful in closed water heating systems. The
system has no source of oxygen , so once all the initial oxygen has reacted,
corrosion is greatly reduced."