DoITPoMS

previous | next

Experimental set-up

 Experimental set-up for measuring creep    Schematic of experimental set-up for measuring creep

In order to create a temperature-controlled environment, the coil is placed inside a Perspex tube. Once the temperature in the tube has stabilised, the coil is allowed to creep under its own weight for one minute. The videos below show qualitatively how creep rate varies with temperature.

Creep deformation of a coil of solder at 28oC
View video of the demonstration (2.96 MB) ... in separate window ... video alone

Creep deformation of a coil of solder at 65oC
View video of the demonstration (3.72 MB) ... in separate window ... video alone

Creep deformation of a coil of solder at 85oC
View video of the demonstration (3.81 MB) ... in separate window ... video alone


previous | next