The equation governing the rate of steady state creep is:
![]()
Q = activation energy; n = stress exponent; A = constant;
This can be rearranged into the form: ![]()
The activation energy Q can be determined experimentally, by plotting the natural log of creep rate against the reciprocal of temperature.

The stress exponent n can be determined by plotting the strain rate as a function of stress.