Batteries Batteries
This TLP investigates the basic principles, design and applications of batteries. It covers both primary and rechargeable batteries, how they work and how they may be used.
Brittle Fracture Brittle Fracture
What determines when a material will break, and whether failure will be catastrophic or more gradual. Cracking is controlled by the energy changes that occur - it is not the stress at the crack tip that is important..
Casting Casting
This TLP introduces a number of important processes through which metallic items can be fabricated from molten metal. As well as detailing the practical aspects of these manufacturing processes, attention is given to the important parameters which determine the microstructure of the finished items.
Crystallinity in Polymers Crystallinity in Polymers
An understanding of polymer crystallinity is important because the mechanical properties of crystalline polymers are different from those of amorphous polymers. Polymer crystals are much stiffer and stronger than amorphous regions of polymer.
Crystallographic Texture Crystallographic Texture
This teaching and learning package (TLP) introduces the concept of texture in crystalline materials such as common metals and metallic alloys.
Diffraction and Imaging Diffraction and Imaging
A brief summary of diffraction and imaging using an optical system.
Examination of a Manufactured Article Examination of a Manufactured Article
This TLP provides an introduction to the deconstruction and investigation of the materials and processes used in an everyday item or article.
Ferroelectric Materials Ferroelectric Materials
Ferroelectrics are an important device in today's world. They are useful both as capacitors, for example in camera flashes, or as non-volatile memory storage. The memory use of which you are most likely to be aware is in the Playstation 2.
Fuel Cells Fuel Cells
This teaching and learning package provides a short summary of four of the most promising fuel cell technologies. It gives a general overview of the field with focus on materials used (electrolytes and electrodes) and the mechanism of function (electrochemistry and thermodynamics).
Indexing Electron Diffraction Patterns Indexing Electron Diffraction Patterns
An introduction to the indexing of diffraction patterns.
The Jominy End Quench Test The Jominy End Quench Test
Discusses the aims, method and use of results of a test for the hardenability of steel.
Materials for Nuclear Power Generation Materials for Nuclear Power Generation
This TLP introduces readers to key challenges in the selection, usage and development of materials for nuclear reactors.
Tags: energy
Microstructural Examination Microstructural Examination
This teaching and learning package (TLP) looks at how what we see in micrographs relates to equilibrium phase diagrams and cooling routes for alloy systems.
Reciprocal Space Reciprocal Space
This TLP shows the construction of reciprocal lattices from real ones, use of the Ewald sphere for diffraction experiments and some other applications of reciprocal space.
The Stereographic Projection The Stereographic Projection
This TLP covers the use of the Stereographic projection and Wulff nets.
X-ray Diffraction Techniques X-ray Diffraction Techniques
This teaching & learning package provides an introduction to X-ray diffraction. It describes the main crystallographic information that can be obtained and experimental methods most commonly used.