The Jominy End Quench Test
This teaching and learning package discusses the Jominy end quench test. It describes the aims of the test and the method of performing the test. It also describes the use of the test data obtained, showing how the data is related to the microstructure produced in a steel sample.
Photograph of Jominy test being carried out
First created: April 2004. "Going further" updated: January 2008. Updated to HTML5: October 2021.