- Labelled diagram of a mounted specimen (image)
- Micrograph of copper specimen ground with 200 grit paper (image)
- Micrograph of copper specimen ground with 400 grit paper (image)
- Micrograph of copper specimen ground with 800 grit paper (image)
- Micrograph of copper specimen ground with 1200 grit paper (image)
- Micrograph of copper specimen polished to 6 micron level (image)
- Micrograph of copper specimen polished to 6 micron level (image)
- Diagrams showing how contrast can arise in microscope image (image)
- Micrograph of etched copper specimen (image)
- Micrograph of over etched copper specimen (image)
- Labelled photograph of specimen levelling press (image)
- Metric graticule in polarised light (image)
- A quartz wedge under crossed polars, (increases in thickness from left to right) so the retardation also increases (image)
- Michel-Levy chart (image)
- Glass ceramic transmission microscope image made with unpolarised light (image)
- Glass ceramic transmission microscope image made with polarised light (image)
- Glass ceramic transmission microscope image made with polarised light and quarter wave plate (image)
- Glass ceramic transmission microscope image made with polarised light and full wave plate (image)
- Diagram illustrating diffraction (image)
- Diagram illustrating diffraction (image)
- Diagram illustrating relationship between numerical aperture and resolution (image)
- Diffraction pattern for unresolvable Airy discs (image)
- Diffraction pattern for Airy discs at the Rayleigh Criterion (image)
- Diffraction pattern for resolvable Airy discs (image)
- Labelled (Flash)
- Labelled rollover diagram of the reflection microscope (Flash)
- Labelled rollover diagram of the transmission microscope (Flash)

© 2004-2012 University of Cambridge.