Warning: you will need a high speed Internet connection to view these videos without a long wait! It takes approximately 6 mins per MB to receive data via a 56K modem. The video clips open in a new window, and can be left to download in the background while you continue using this window.
The videos of the experiment are in QuickTime format and require your browser to have the QuickTime plugin installed. If necessary download the plugin from the QuickTime download site.
3-point bending
Normal bar
Annealed
bar undergoing 3-point bending under a circular polariscope (2.6 MB) ... in separate window ... video alone
Close
up of the same (2.3 MB) ... in separate window ... video alone
Abaqus-generated
simulation of a bar undergoing 3-point bending (87 KB) ... in separate window ... video alone
Bar with Notch
Annealed
bar with notch undergoing 3-point bending under a circular polariscope (2.8 MB) ... in separate window ... video alone
Abaqus-generated
simulation of a bar with notch undergoing 3-point bending (94 KB) ... in separate window ... video alone
Bar with Hole
Annealed
bar with hole undergoing 3-point bending under a circular polariscope (2.5 MB) ... in separate window ... video alone
Abaqus-generated
simulation of a bar with hole undergoing 3-point bending (96 KB) ... in separate window ... video alone
4-point bending
Normal bar
Annealed
bar undergoing 4-point bending under a circular polariscope (2.6 MB) ... in separate window ... video alone
Close
up of the same (2.4 MB) ... in separate window ... video alone
Abaqus-generated
simulation of a bar undergoing 4-point bending (94 KB) ... in separate window ... video alone
Bar with Notch
Annealed
bar with notch undergoing 4-point bending under a circular polariscope (2.2 MB) ... in separate window ... video alone
Abaqus-generated
simulation of a bar with notch undergoing 4-point bending (99 KB) ... in separate window ... video alone
Bar with Hole
Annealed
bar with hole undergoing 4-point bending under a circular polariscope (2.4 MB) ... in separate window ... video alone
Abaqus-generated
simulation of a bar with hole undergoing 4-point bending (102 KB) ... in separate window ... video alone