DoITPoMS Video Library Full Record for Video 145

Full Record for Video 145

Click to view video 145
[16 sec, audio: No]

View video in new window

Download
Windows media file [1520 Kb]
Quicktime video [924 Kb]
video no
145
Brief description
A force is applied to a paper sheet by stretching it across a metal strip. When the cut is lengthened the crack grows quite suddenly. From TLP: Brittle Fracture
Categories
Experimental procedure