Brief description
Part of a series of videos showing the glass transition in polymers, and the resulting change in energy dissipation on impact: Video at one tenth actual speed of a rubber ball bouncing at -70° C (close to Tg), showing that nearly all the energy is dissipated, and the ball barely bounces at all. From TLP The Glass Transition in Polymers