Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Video Library Full Record for Video 44

Full Record for Video 44

Click to view video 44
[16 sec, audio: No]

View video in new window

Download
Windows media file [1692 Kb]
Quicktime video [1142 Kb]
video no
44
Brief description
Video of the tranferral of a steel specimen from furnace to water jet during a jominy end quench test. The steel is held in a furnace to austenitise the microstructure at around 900ºC. It is then transferred to the quenching machine where a water jet is sprayed onto the bottom of the specimen until the specimen is cool. From TLP: The Jominy End Quench Test
Categories
Experimental procedure
Date
09/08/06
Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International

You can also view this video on YouTube