DoITPoMS Video Library Full Record for Video 66

Full Record for Video 66

Click to view video 66
[7 sec, audio: No]

View video in new window

Download
Windows media file [461 Kb]
Quicktime video [340 Kb]
video no
66
Brief description
Animation of slip by the movement of an edge dislocation.
Categories
Atomistic animations
Date
10/08/06
Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International

You can also view this video on YouTube