DoITPoMS Video Library Full Record for Video 79

Full Record for Video 79

Click to view video 79
[25 sec, audio: No]

View video in new window

Download
Windows media file [2779 Kb]
Quicktime video [3817 Kb]
video no
79
Brief description
A coil of solder creeping under its own weight at 85 °?C. From TLP Creep deformation of metals