Browse the Library
Categories > Metal or alloy > Bi-Cd
4 micrographs available, ordered by micrograph number.
Micrograph
6
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
7
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
8
:
Bi 80, Cd 20 (wt%), hypereutectic alloy System: Bi-Cd, Composition: Bi 80, Cd 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
9
:
Bi 80, Cd 20 (wt%), hypereutectic alloy System: Bi-Cd, Composition: Bi 80, Cd 20 (wt%) Reflected light microscopy 80 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.