Categories > Metal or alloy > Ni-X

4 compositions available. The number of micrographs available is given in [brackets].


Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al [8]
Show relevant: techniques, keywords, micrographs

Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy) [3]
Show relevant: techniques, keywords, micrographs

Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) [7]
Show relevant: techniques, keywords, micrographs

Not specified (Ni-Superalloy) [3]
Show relevant: techniques, keywords, micrographs