DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Metal or alloy > Scanning electron microscopy (SEM)

48 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 48 micrographs Page 1 2 3 4 5 | Previous | Next

Link to full record for micrograph 2 Micrograph 2 : Al 75, Cu 25 (wt%), hypoeutectic alloy
System: Al-Cu, Composition: Al 75, Cu 25 (wt%)
Scanning electron microscopy (SEM)
30 μm
Link to full record for micrograph 4 Micrograph 4 : Al 67, Cu 33 (wt%), eutectic alloy
System: Al-Cu, Composition: Al 67, Cu 33 (wt%)
Scanning electron microscopy (SEM)
15 μm
Link to full record for micrograph 19 Micrograph 19 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Scanning electron microscopy (SEM)
30 μm
Link to full record for micrograph 20 Micrograph 20 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 23 Micrograph 23 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 24 Micrograph 24 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 28 Micrograph 28 : Fe, C 0.9 (wt%), martensite
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 53 Micrograph 53 : Cu 60, Zn 40 (wt%), quenched and held at 300°C - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Scanning electron microscopy (SEM)
15 μm
Link to full record for micrograph 75 Micrograph 75 : Notched zinc, broken by impact at room temperature
System: Zn, Composition: Notched zinc
Scanning electron microscopy (SEM)
1 mm
Link to full record for micrograph 76 Micrograph 76 : Notched zinc, broken by impact at room temperature
System: Zn, Composition: Notched zinc
Scanning electron microscopy (SEM)
160 μm