134
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 600 nm |
|
Micrograph
135
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 1.5 μm |
|
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
|
Micrograph
614
:
Rapid solidification in an atomised droplet System: Al-Mg, Composition: Al 90, Mg 10 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
723
:
Ni-Superalloy System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy) Transmission electron microscopy (TEM) 200 nm |
|
Micrograph
772
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
773
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
774
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
775
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
776
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 2 μm |