Link to full record for micrograph 558 Micrograph 558 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB
Transmitted light microscopy
20 μm
Link to full record for micrograph 596 Micrograph 596 : Glass-fibre reinforced polymer
System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres
Reflected light microscopy
400 μm
Link to full record for micrograph 602 Micrograph 602 : Section of a metal matrix composite (MMC)
System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%)
Reflected light microscopy, polarised
80 μm
Link to full record for micrograph 603 Micrograph 603 : Section of a metal matrix composite (MMC)
System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%)
Reflected light microscopy, polarised
80 μm
Link to full record for micrograph 606 Micrograph 606 : Extruded Saffil-containing metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 619 Micrograph 619 : Tensile failure surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix