Browse the Library
Categories > Polymer > Keyword: carbon
10 micrographs available, ordered by micrograph number.
Micrograph
561
:
Ordered film of carbon nanotubes System: Carbon nanotube, Composition: Not specified Field emission gun scanning electron microscopy (FEGSEM) 400 nm |
|
Micrograph
562
:
Multi-walled carbon nanotube System: Carbon nanotube, Composition: Not specified Transmission electron microscopy (TEM) 3.2 nm |
|
Micrograph
563
:
Carbon nanotubes System: Carbon nanotube, Composition: Low concentration (<0.3 vol%) suspension in water Field emission gun scanning electron microscopy (FEGSEM) 99 nm |
|
Micrograph
564
:
Aligned array of nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 25 μm |
|
Micrograph
565
:
Vapour-grown carbon nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 5 μm |
|
Micrograph
594
:
Carbon string System: C, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
|
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
|
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
|
Micrograph
643
:
Aligned carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 1 μm |
|
Micrograph
644
:
Carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 100 nm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.