Link to full record for micrograph 561 Micrograph 561 : Ordered film of carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Field emission gun scanning electron microscopy (FEGSEM)
400 nm
Link to full record for micrograph 562 Micrograph 562 : Multi-walled carbon nanotube
System: Carbon nanotube, Composition: Not specified
Transmission electron microscopy (TEM)
3.2 nm
Link to full record for micrograph 563 Micrograph 563 : Carbon nanotubes
System: Carbon nanotube, Composition: Low concentration (<0.3 vol%) suspension in water
Field emission gun scanning electron microscopy (FEGSEM)
99 nm
Link to full record for micrograph 564 Micrograph 564 : Aligned array of nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
25 μm
Link to full record for micrograph 565 Micrograph 565 : Vapour-grown carbon nanotubes
System: Carbon nanotube, Composition: Not specified
Scanning electron microscopy (SEM)
5 μm
Link to full record for micrograph 566 Micrograph 566 : Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 567 Micrograph 567 : Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 568 Micrograph 568 : Strain induced birefringence in a thermoformed PET cup
System: Polyethylene terephthalate (PET), Composition: Not specified
Cross-polarised light microscopy
8 mm
Link to full record for micrograph 569 Micrograph 569 : Injection-moulded polystyrene ruler
System: Polystyrene (PS), Composition: Not specified
Cross-polarised light microscopy
11 mm
Link to full record for micrograph 570 Micrograph 570 : Strain-induced birefringence in a notched polycarbonate bar
System: Polycarbonate (PC), Composition: Not specified
Cross-polarised light microscopy
6 mm