614
:
Rapid solidification in an atomised droplet System: Al-Mg, Composition: Al 90, Mg 10 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
615
:
Cross-section of an aluminium casting System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy 10 mm |
|
Micrograph
616
:
Cavity formation in a tensile loaded alumina particulate composite System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles Scanning electron microscopy (SEM) 80 μm |