320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 311 - 320 of 320 micrographs | Page 1 .. 26 27 28 29 30 31 32 | Previous | Next |
![]() |
Micrograph
528
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
529
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
530
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
531
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
532
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
533
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
534
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 800 μm |
![]() |
Micrograph
535
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
536
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
537
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 100 μm |