Link to full record for micrograph 557 Micrograph 557 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 15%PB
Transmitted light microscopy
10 μm
Link to full record for micrograph 558 Micrograph 558 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB
Transmitted light microscopy
20 μm
Link to full record for micrograph 559 Micrograph 559 : Shear bands in stressed polycarbonate
System: Polycarbonate (PC), Composition: Not specified
Scanning electron microscopy (SEM)
800 μm
Link to full record for micrograph 560 Micrograph 560 : Crazing near a fracture surface in polystyrene
System: Polystyrene (PS), Composition: Not specified
Photography (no microscope)
10 mm
Link to full record for micrograph 568 Micrograph 568 : Strain induced birefringence in a thermoformed PET cup
System: Polyethylene terephthalate (PET), Composition: Not specified
Cross-polarised light microscopy
8 mm
Link to full record for micrograph 569 Micrograph 569 : Injection-moulded polystyrene ruler
System: Polystyrene (PS), Composition: Not specified
Cross-polarised light microscopy
11 mm
Link to full record for micrograph 570 Micrograph 570 : Strain-induced birefringence in a notched polycarbonate bar
System: Polycarbonate (PC), Composition: Not specified
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 571 Micrograph 571 : Strain-induced birefringence in a polycarbonate bar
System: Polycarbonate (PC), Composition: Not specified
Cross-polarised light microscopy
14 mm
Link to full record for micrograph 572 Micrograph 572 : Birefringence in a film of polypropylene
System: Polypropylene (PP), Composition: Not specified
Cross-polarised light microscopy
10 mm
Link to full record for micrograph 573 Micrograph 573 : Birefringence in a film of polyethylene
System: Low density polyethylene (LDPE), Composition: Not specified
Cross-polarised light microscopy