6 micrographs for keyword clay, ordered by micrograph number.
![]() |
Micrograph
177
:
Terracotta pottery System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 200 μm |
![]() |
Micrograph
178
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 100 μm |
![]() |
Micrograph
179
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 250 μm |
![]() |
Micrograph
187
:
Part of a Denby pottery mug, showing the glaze on the surface System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
![]() |
Micrograph
188
:
Part of a Denby pottery mug System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
![]() |
Micrograph
190
:
Aluminous Electrical Porcelain System: Triaxial (i.e. clay/flux/filler) porcelain, Composition: Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%) Scanning electron microscopy (SEM) 10 μm |