Keyword
274 micrographs for keyword carbon, ordered by micrograph number.
Showing 231 - 240 of 274 micrographs | Page 1 .. 21 22 23 24 25 26 27 28 | Previous | Next |
Micrograph
412
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
413
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
414
:
Cast iron, containing phosphorus System: Fe-C-X, Composition: Fe, C 3.46, Si 0.12, Mn 0.33, P 1.91, Cr 1.02 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
415
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 800 μm |
|
Micrograph
416
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
|
Micrograph
417
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy, polarised with wave-plate 800 μm |
|
Micrograph
418
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
419
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
|
Micrograph
561
:
Ordered film of carbon nanotubes System: Carbon nanotube, Composition: Not specified Field emission gun scanning electron microscopy (FEGSEM) 400 nm |
|
Micrograph
562
:
Multi-walled carbon nanotube System: Carbon nanotube, Composition: Not specified Transmission electron microscopy (TEM) 3.2 nm |
Showing 231 - 240 of 274 micrographs | Page 1 .. 21 22 23 24 25 26 27 28 | Previous | Next |