Micrograph 39 and full record

- Micrograph no
- 39
- Brief description
- Cu 98, Be 2 (wt%), quenched and aged - annealing twins
- Keywords
- alloy
, annealing
, beryllium, copper, metal, quenching
, solution heat treatment
, twinning
- Categories
- Metal or alloy
- System
- Cu-Be
- Composition
- Cu 98, Be 2 (wt%)
- Standard codes
- Reaction
- Processing
- Solution treated, quenched and aged
- Applications
- Sample preparation
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- This sample was solution treated, quenched and aged. Recrystallisation occurs during ageing creating annealing twins.
- Contributor
- Prof T W Clyne
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 25/10/01
- Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales