Micrograph 497 and full record
- Micrograph no
- 497
- Brief description
- Cu 90, Sn 10 (wt%) bronze, cast annealed
- Keywords
- alloy , annealing , bronze , copper, metal, tin
- Categories
- Metal or alloy
- System
- Cu-Sn
- Composition
- Cu 90, Sn 10 (wt%)
- Standard codes
- Reaction
- Processing
- Cast annealed 500 ºC and air cooled
- Applications
- Sample preparation
- Ferric chloride
- Technique
- Reflected light microscopy
- Length bar
- 800 μm
- Further information
- Bronze annealed at a temperature sufficient to cause grain growth in the alloy. This can be seen in the large grain sizer present in the sample.
- Contributor
- Dr R F Cochrane
- Organisation
- Department of Materials, University of Leeds
- Date
- 04/09/02
- Licence for re-use
- Attribution-NonCommercial-ShareAlike 4.0 International
- Related micrographs
View image alone .. in a new window
Help is available on downloading images