Micrograph 590 and full record
- Micrograph no
- 590
- Brief description
- Remnants of crazes on a polycarbonate fracture surface
- Keywords
- craze , craze remnants, fibril , fracture , polycarbonate (PC), polymer
- Categories
- Fracture, Polymer
- System
- Polycarbonate (PC)
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Applications
- Polycarbonate is a clear and relatively tough plastic used to make shatterproof windows, lenses and even helmets. It is also used to make compact discs.
- Sample preparation
- The surface has been sputter-coated with gold, to give a conducting surface
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 10 μm
- Further information
- The fracture surface shows fibrils of oriented polymer which are the remnants of crazes. Crazes are both a precursor to cracking and a toughening mechanism in stressed polymers. They only form when a certain critical tensile stress has been attained and form perpendicular to the largest tensile principal stress. They are very fine crack-like projections from the fracture surface but are bridged by even finer material, giving approximately 50% voids. It is these fibrils which interfere with light in an otherwise transparent polymer to make the crazing visible as a whitening of the strained material. It is the remnants of these fibrils which are visible on this fracture surface.
- Contributor
- J A Curran
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 03/10/02
- Licence for re-use
- Attribution-NonCommercial-ShareAlike 4.0 International
- Related micrographs
View image alone .. in a new window
Help is available on downloading images