DoITPoMS

System

2 micrographs for system Cu-Ni, ordered by micrograph number.


Link to full record for micrograph 10 Micrograph 10 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 11 Micrograph 11 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
80 μm

List all systems