Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

System
64 micrographs for system Cu-Zn, ordered by micrograph number.
Showing 11 - 20 of 64 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
50
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
51
:
Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
52
:
Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
53
:
Cu 60, Zn 40 (wt%), quenched and held at 300°C - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Scanning electron microscopy (SEM) 15 μm |
![]() |
Micrograph
420
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
421
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
422
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
423
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
424
:
Commercial brass, ~30% Zn, displaying dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
425
:
Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure) Reflected light microscopy 800 μm |
Showing 11 - 20 of 64 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |