Technique
564 micrographs for technique Reflected light microscopy, ordered by micrograph number.
Showing 91 - 100 of 564 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 57 | Previous | Next |
Micrograph
187
:
Part of a Denby pottery mug, showing the glaze on the surface System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
|
Micrograph
188
:
Part of a Denby pottery mug System: Al2O3-SiO2, Composition: Mostly clay (which consists of alumina and silica) Reflected light microscopy 200 μm |
|
Micrograph
193
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
|
Micrograph
194
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
|
Micrograph
198
:
96% Alumina System: Al2O3, Composition: Al2O3 96%, remainder MgO, CaO, SiO2 Reflected light microscopy 250 μm |
|
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
|
Micrograph
202
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 200 μm |
|
Micrograph
203
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
204
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
205
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
Showing 91 - 100 of 564 micrographs | Page 1 .. 7 8 9 10 11 12 13 .. 57 | Previous | Next |