Link to full record for micrograph 928 Micrograph 928 : Edo time japanese sword
System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%)
Reflected light microscopy
2 mm
Link to full record for micrograph 929 Micrograph 929 : Edo time japanese sword
System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 931 Micrograph 931 : Afunfun, Niger. Melilith-pyroxene-copper slag
System: Cu production, Composition: Not specified
Reflected light microscopy
200 μm
Link to full record for micrograph 932 Micrograph 932 : Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène)
System: Smithing slag, Composition: Not specified
Reflected light microscopy
500 μm
Link to full record for micrograph 934 Micrograph 934 : Experimental iron production, Ph. Andrieux, Paris
System: Fe production, Composition: Not specified
Reflected light microscopy
500 μm
Link to full record for micrograph 935 Micrograph 935 : Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag
System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%)
Reflected light microscopy
2 mm
Link to full record for micrograph 937 Micrograph 937 : Fernando Lopez (Sierra Alhamilla), Almería, Spain
System: Cu production, Composition: Not specified
Reflected light microscopy
500 μm
Link to full record for micrograph 938 Micrograph 938 : Fernando Lopez (Sierra Alhamilla), Almería, Spain
System: Cu production, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 940 Micrograph 940 : Morro-de-Mezquitilla, Malaga, Spain. Iron smithing slag
System: Smithing slag, Composition: Not specified
Reflected light microscopy
500 μm
Link to full record for micrograph 941 Micrograph 941 : Nakhlak, Central Iran. Lead production slag
System: Pb, Composition: Not specified
Reflected light microscopy
500 μm