Technique
564 micrographs for technique Reflected light microscopy, ordered by micrograph number.
Showing 61 - 70 of 564 micrographs | Page 1 .. 4 5 6 7 8 9 10 .. 57 | Previous | Next |
Micrograph
69
:
Grey cast iron core with white cast iron periphery System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 40 μm |
|
Micrograph
70
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 200 μm |
|
Micrograph
71
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 80 μm |
|
Micrograph
72
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 400 μm |
|
Micrograph
73
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 80 μm |
|
Micrograph
84
:
Alumina System: Alumina, Composition: Not specified Reflected light microscopy 800 μm |
|
Micrograph
85
:
Alumina System: Alumina, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
129
:
Woven E - glass fibres in a DERAKANE (TM) matrix System: Glass fibre composite, Composition: Not specified Reflected light microscopy 800 μm |
|
Micrograph
130
:
Woven E - glass fibres in a DERAKANE (TM) matrix System: Glass fibre composite, Composition: Not specified Reflected light microscopy 200 μm |
|
Micrograph
131
:
Unidirectional T800 carbon fibres in an MTM49 epoxy matrix. System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
Showing 61 - 70 of 564 micrographs | Page 1 .. 4 5 6 7 8 9 10 .. 57 | Previous | Next |