Technique
564 micrographs for technique Reflected light microscopy, ordered by micrograph number.
Showing 81 - 90 of 564 micrographs | Page 1 .. 6 7 8 9 10 11 12 .. 57 | Previous | Next |
Micrograph
167
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
168
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
|
Micrograph
169
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 40 μm |
|
Micrograph
175
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 100 μm |
|
Micrograph
176
:
Concrete from a commercial paving slab System: Concrete, Composition: Aggregate, cement, water Reflected light microscopy 250 μm |
|
Micrograph
177
:
Terracotta pottery System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 200 μm |
|
Micrograph
178
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 100 μm |
|
Micrograph
179
:
Terracotta pottery, showing the glaze on the surface System: Terracotta, Composition: Terracotta is composed of mixtures of fired grog and clay. Reflected light microscopy 250 μm |
|
Micrograph
185
:
Silicon Nitride-bonded Silicon Carbide System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 250 μm |
|
Micrograph
186
:
Silicon Carbide from within a Silicon Nitride-bonded Silicon Carbide sample System: Silicon nitride-bonded silicon carbide, Composition: Particles of SiC in a reaction-bonded Si3N4 matrix Reflected light microscopy 25 μm |
Showing 81 - 90 of 564 micrographs | Page 1 .. 6 7 8 9 10 11 12 .. 57 | Previous | Next |