133
:
Steel, austenitised at 1200 centigrade for 120 s and then transformed isothermally at 350 centigrade for 2000 s before cooling to room temperature. System: Fe-C-X, Composition: Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%) Atomic force microscopy (AFM) 1 μm |
![]() |
Micrograph
646
:
Spherulite growth imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 500 nm |
![]() |
Micrograph
647
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 3 μm |
![]() |
Micrograph
648
:
A spherulite imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 2 μm |
![]() |
Micrograph
649
:
An image of an alkane crystal taken by AFM System: Alkane, Composition: C36H74 Atomic force microscopy (AFM) 30 μm |
![]() |
Micrograph
850
:
Stainless Steel 430. System: Fe-C-X, Composition: Stainless steel 430 Atomic force microscopy (AFM) 20 μm |
![]() |
Micrograph
851
:
Polystyrene System: Polystyrene (PS), Composition: Polystyrene Atomic force microscopy (AFM) 2 μm |
![]() |
Micrograph
852
:
Polystyrene System: Polystyrene (PS), Composition: Polystyrene Atomic force microscopy (AFM) 200 nm |
![]() |
Micrograph
853
:
Colloidal polymethyl methacrylate System: Poly methyl methacrylate, Composition: Poly methyl methacrylate Atomic force microscopy (AFM) 200 nm |
![]() |
Micrograph
857
:
Low Carbon Steel System: Fe-C-X, Composition: Fe, C low (wt%) Atomic force microscopy (AFM) 20 μm |