Technique
21 micrographs for technique Atomic force microscopy (AFM), ordered by micrograph number.
Showing 21 of 21 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
871
:
Low Carbon Steel System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Atomic force microscopy (AFM) 30 μm |
Showing 21 of 21 micrographs | Page 1 2 3 | Previous | Next |