Micrograph
160
:
Glass ceramic, heat treated at 750° C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
162
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
164
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
170
:
ZnO varistor System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
171
:
ZnO varistor System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
172
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
173
:
Bone china, showing the glaze on the surface (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
174
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
180
:
Oven-to-tableware showing the glaze on the surface, using a sensitive tint plate System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 200 μm |
![]() |
Micrograph
181
:
Oven-to-tableware System: Miscellaneous, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |