Technique
14 micrographs for technique Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode, ordered by micrograph number.
Showing 11 - 14 of 14 micrographs | Page 1 2 | Previous | Next |
Micrograph
730
:
Magnesium alloy System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 200 μm |
|
Micrograph
731
:
Metal matrix composite of magnesium and alumina fibres System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy), reinforced with Alumina fibres with a volume fraction of 14% Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
|
Micrograph
732
:
Magnesium alloy System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 200 μm |
|
Micrograph
733
:
Magnesium alloy, fracture surface System: Mg-Zn, Composition: Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 20 μm |
Showing 11 - 14 of 14 micrographs | Page 1 2 | Previous | Next |