Technique
87 micrographs for technique Scanning electron microscopy (SEM), ordered by micrograph number.
Showing 31 - 40 of 87 micrographs | Page 1 2 3 4 5 6 7 .. 9 | Previous | Next |
Micrograph
147
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
190
:
Aluminous Electrical Porcelain System: Triaxial (i.e. clay/flux/filler) porcelain, Composition: Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%) Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
548
:
Fractograph showing extensive matrix cracking and fibres bridging an opened matrix in a fibre reinforced magnesium aluminosilicate ceramic System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
559
:
Shear bands in stressed polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
|
Micrograph
564
:
Aligned array of nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 25 μm |
|
Micrograph
565
:
Vapour-grown carbon nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 5 μm |
|
Micrograph
579
:
SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
|
Micrograph
580
:
High magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
|
Micrograph
582
:
Low magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 4 mm |
|
Micrograph
583
:
SEM image of Velcro (TM) System: Nylon, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |